Beilstein J. Nanotechnol. 2014, 5, 596–602, doi:10.3762/bjnano.5.70
Figure 1: Photo of the dual chamber ALL-oxide MBE system installed in the Max-Planck Institute for Solid Stat...
Figure 2: Sketch of the growth chamber.
Figure 3: AFM image of 25 nm thick La2NiO4 film on STO substrate.
Figure 4: AFM image of 25 nm thick La2CuO4 film on LSAO substrate.
Figure 5: XRD θ–2θ scan of a bilayer heterostructure La2NiO4 (diamonds)–La2CuO4 (circles) on a STO(100) subst...
Figure 6: Resistivity versus temperature for the parent compound La2CuO4 and for the superconducting La2CuO4+δ...
Figure 7: XRD θ–2θ scan of 13 nm thick La1Sr1NiO4 on LSAT(100) (S). Laue fringes can be seen in the left inse...
Figure 8: Resistivity versus temperature for La2−xSrxNiO4 with different doping levels.